Liquid Phase Photo-Polymerization

  • Materials: Glass slides HybriWell gasketed polycarbonate film Photomask Prepolymer mixture (92 wt.% isobornyl acrylate, 5 wt.% tetraethyleneglycol dimethacrylate, 3 wt.% 2,2A-dimethoxy-2- phenyl-acetophenone) UV lamp
  • Protocol: Fill with prepolymer mixture: isobornyl acrylate, tetraethyleneglycol dimethacrylate (x-linker), 2,2A-dimethoxy-2-phenyl-acetophenone (photoinitiator) Suction off uncured prepolymer. Rinse with EtOH and water. Glue inlets/outlets (blunt suringe needles) via 5-min epoxy.

<p>Hi</p><p>Thank you! No I am at student, it's one of my lab reports for a very good course in microfluidics I took last summer (see link below) </p><p><a href="http://www.summer.harvard.edu/courses/introduction-fabrication-microfluidic-devices" rel="nofollow">http://www.summer.harvard.edu/courses/introduction...</a></p>
<p>This looks interesting.</p><p>Are you a teacher, and this a guide for your students?</p>

About This Instructable

288views

1favorite

License:

More by gcannici:Paper Microfluidic Devices Liquid Phase Photo-Polymerization Microcontact Printing 
Add instructable to: