PCB Etching Solution - Cupric Chloride by vkoudymov
Featured

Step 2: Pour Acid & Clean Copper

01A - Acid Measurement & Container.jpg
01B - Acid Color.jpg
01C - Acid Wash of Copper.jpg
01D - Water Wash of Copper.jpg
1. Pour about 11 oz. muriatic acid (25% hydrochloric acid) into a glass jar, its color should be clear.
2. Carefully place the cooled piece of oxizided copper into the jar, it will change the acid a yellow-green color.
3. Place the copper into a bowl of water to clean it, set the acid aside.
 