Plastic PE add PS
20khz frequency welder
20psi sealing 20s

Step 1: Setup Fixtures

Step 2: Set Parameters

Energy model 180j
30psi
Hold time 0.3
Amplitude 100 50umm

Step 3: Welded

Step 4: Testing

Sealing the hole, put 20ps to the product. But... Failed

Step 5: Change Parameter

Add energy